Inqubo yokushisela yepayipi lokuphakela amanzi le-PE

Ukunikezwa kwamanzi kwe-PEIzinyathelo zenqubo yokushisela ipayipi:

1) Ngokuya ngemininingwane yokushisela yepayipi lokuhambisa amanzi le-PE, khetha isikhunta sokushisela bese uvula ukushisisa kukagesi:

2) Ngokushintsha kwezinga lokushisa lesizini, izinga lokushisa liyashintshashintsha noma lehle (±10 ℃) lisuka ezingeni lokushisa elijwayelekile lasekuqaleni, izinga lokushisa elijwayelekile lingu-20 ℃

3) Nciphisa ubuso bokugcina bepayipi lokuhlinzeka ngamanzi le-PE ukuze ubuso balo bokuphela buhambisane ne-eksisi;

4) Ipayipi lokuphakela amanzi kanye nokufakwa kwamapayipi kufanele kugcine ukuphazamiseka okufanele, futhi ingxenye engaphezulu kufanele isuswe ngamathuluzi okusika.

5) Khipha ukungcola nokunye ukungcola ezindaweni ezingaphandle nangaphakathi zezindawo zokushisela zamapayipi okuhambisa amanzi kanye nezinto zokufakelwa.

I-6) Enqubweni yokushisela, ukujula kokufakwa kwepayipi lokuhambisa amanzi akufanele kujule kakhulu, okuzobangela ukuvinjelwa kwepayipi lokuhambisa amanzi, elingafaneleki ukutshuza, i-diving welding ingase ingaqini.

7) Faka ipayipi lokuphakela amanzi elishiselwe le-PE kanye nepayipi elifaka endaweni yokufudumeza ngesikhathi esifanayo.Lapho isikhathi sokushisa sifinyelelwa, khipha ngokushesha bese ufaka umkhawulo oshiselwe wepayipi lokuhambisa amanzi epayipini elihambisana nokucindezela okufanayo (ngokuvamile i-2-3 Mpa).Phusha kuze kufakwe ukujula okumakiwe epayipini, okuvumela uhla oluncane lokulungiswa ngesikhathi esifushane kakhulu.

8) Ngokuvumelana nemininingwane yepayipi lokuphakela amanzi le-PE, gcina isimo sokushisela ngesikhathi sokupholisa, ngokuvamile sisuka kumizuzu engama-30 kuye kwengama-50.